MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-OP230 E&E Equipment Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEM-OP SERIES is no doubt to be the first choice for E&E equipment to meet the various fire classes. With high decomposition temperature, GOYENCHEM-OP SERIES provides your E&E equipment products excellent flame retard ablity. GOYENCHEM-OP SERIES , an innovative flame retardant products with tiny particle size provide the best solution ever for your E&E equipment products.

Intro: GOYENCHEM-OP SERIES is no doubt to be the first choice for E&E equipment to meet the various fire classes. With high decomposition temperature, GOYENCHEM-OP SERIES provides your E&E equipment products excellent flame retard ablity. GOYENCHEM-OP SERIES , an innovative flame retardant products with tiny particle size provide the best solution ever for your E&E equipment products.

Advantages:

  • Goyenchem-OP95 owns thin particles.
  • Goyenchem-OP312 offer prominent fireproof ability.
  • Goyenchem-OP230 with perfect heat-resistance and anti heat decomposition.
  • Insoluble in water and general organic solvent.
  • With outstanding water resistance
  • With anti-ion migration ability and comprehensive mechanical properties
  • With excellent electrical and mechanical properties.
  • With high effective phosphorus element.
  • With outstanding dispersion in resin and organic solvent.
  • Modified the comprehensive properties of polymer and enhance the fireproof ability.
Applications:
  • High temperature polyamides
  • Polyamide compounds
  • Glass-fiber-reinforced and unreinforced grades.
  • Various kind of thermoplastic and thermosetting type resins
  • Epoxy resin electronics potting compounds
  • Epoxy-based printed circuit board (PCB)
  • Flexible flame retard copper clad laminate (FR-FCCL) and flame retard copper clad laminate (FR-CCL)
  • Various kinds of high end Electrical and Electronic (E&E) Equipment applications.
  • Thermoplastic and thermosetting type resins and elastomer such as PET, PBT, PP, TPU, Nylon, SEBS and so on.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 350 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 23.2 - 24 %
 
Descriptive Properties
AppearanceWhite fine powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN017 / 266325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.