MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials TSE392 One Component RTV Adhesive Sealant/Coating, Clear/White  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials incorporate a newly developed crosslinking chemistry and are non-corrosive to metallic substrates. They are particularly well suited for electrical/electronic applications.

This series of products differ in consistency, TSE392 is a thixotropic paste, TSE397 is semi-flowable, and TSE399 is flowable. When cured, they retain their elastomeric properties throughout the operating range of temperature from -55C to 200°C (-67F to 392F).

Product Features:

  • Meets the corrosion resistant requirements of MIL-A-46146A
  • Fast cure at ambient temperatures
  • Odor, slight alcohol
  • Outstanding adhesion, including most plastics
  • Outstanding electrical properties
  • Resistant to heat, cold, moisture, UV, ozone and chemicals

Product Benefits:

  • One component, no mixing or de-airing required
  • Soft consistency provides protection against mechanical and thermal shock
  • Excellent electrical insulation
  • Protects against moisture
  • Varying viscosities allow thorough coating around complex assemblies (TSE399) and thicker coatings where required i.e., high voltage components (TSE392 & TSE397).
  • Convenient packaging/dispensing tubes or cartridges.

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30
Tensile Strength, Ultimate 16.0 kg(f)/cm²
Elongation at Break 400 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cm
Dielectric Constant 2.9
@Frequency 60 Hz
Dielectric Strength 22.0 kV/mm
Dissipation Factor 0.0050
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 0.0833 hour
 
Descriptive Properties
ColorClear/White
ConsistencyThixotropic paste

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Momentive Performance Materials TSE399 One Component RTV Adhesive Sealant/Coating, Clear/White/Black
Momentive Performance Materials TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White
Momentive Performance Materials TSE3282-G Thermally Conductive Silicone Adhesive
Momentive Performance Materials TSE3281G Thermally Conductive, Heat Cured Silicone Adhesive

PGESIL072 / 41063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.