MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Silfoam® SC 203 FOOD GRADE Silicone Antifoam Compound
Categories: Fluid

Material Notes: Product description: SILFOAM® SC 203 FOOD GRADE is a 100% actives solvent dispersible silicone compound designed to control foam in both aqueous and non-aqueous foaming systems. It can be easily emulsified for use in aqueous systems. SILFOAM® SC 203 FOOD GRADE contains those ingredients which conform to the FDA requirements as published in the CODE OF FEDERAL REGULATIONS. (Under Title 21 "Food and Drugs," Part 173, "Secondary Direct Food Additives Permitted in Food for Human Consumption," Paragraph 173.340 "Defoaming Agents".) Because this regulation contains limitations, compliance to the regulation is the responsibility of the law. SILFOAM® SC 203 FOOD GRADE also meets other FDA guidelines. When SILFOAM® SC 203 FOOD GRADE is used directly in food products or for food processing, the maximum amount of silicone permitted should be 10 ppm silicone or 10 ppm SILFOAM® SC 203 FOOD GRADE. Rinsing food with copious amounts of fresh potable water is required after processing. SILFOAM® SC 203 FOOD GRADE meets NSF Category Code 3D-it is acceptable for use in meat, poultry and other food processing areas, when used to wash fruits and vegetables that will become ingredients in meat, poultry and rabbit products. After use, the fruits and vegetables must be rinsed thoroughly in potable water. SILFOAM® SC 203 FOOD GRADE also meets NSF Category Code Q5 (for use in egg washing machines). Shell eggs using this material must be immediately rinsed in warm potable water containing an EPA registered sanitizer. In both NSF instances, the maximum amount of silicone permitted should be 10 ppm (ie. 10 ppm SILFOAM® SC 203 FOOD GRADE) in the final food product SILFOAM® SC 203 FOOD GRADE also can be used in agricultural applications, regulated by the Environmental Protection Agency (EPA). The material meets 40CFR 180.1001(c) and -(d) criteria. SILFOAM® SC 203 FOOD GRADE can also be used in various industrial and consumer applications. The amount of SILFOAM® SC 203 FOOD GRADE required is best determined by trial and error in the actual working conditions. Levels required may vary from a few ppm to 100 ppm, depending upon the severity of the situation.

Application: It is recommended that SILFOAM® SC 203 FOOD GRADE be stirred under low shear for a few minutes before using. This will ensure that the fillers are completely dispersed in the material. SILFOAM® SC 203 FOOD GRADE is most efficient if introduced into the system before foaming has begun. SILFOAM® SC 203 FOOD GRADE may be introduced as is by dispersing in one or more of the ingredients of the system in which foam is to be controlled. An alternate method is to disperse the SILFOAM® SC 203 FOOD GRADE in an appropriate solvent and then add this dispersion to the system in which foam control is desired diluents

  • Aromatic hydrocarbons – toluene
  • Aliphatic hydrocarbons - mineral spirits, t-butanol
  • Esters
Note: If solvents are used to aid dispersing the SILFOAM® SC 203 FOOD GRADE, the FDA and food contact sanctioning becomes null and void.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Viscosity 1500 - 3700 cP
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Active ingredients (%)100
AppearanceGray opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Silfoam® SE 23 FOOD GRADE Silicone Antifoam Emulsion
Dow XIAMETER® PMCPPMX-200 350CS Food Grade Silicone Fluid
Wacker Wacker® AK 350 Food Grade/Kosher Silicone Fluid
Wacker Wacker® AK 1000 US Food Grade/Kosher Silicone Fluid
Wacker Silfoam® SE 21 FOOD GRADE Silicone Antifoam Emulsion

PWACK9440 / 204969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.