MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Pyrotek TS-550 Insulating Board
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the forming versatility and uniform material composition of engineering plastics.

Applications

  • Container glass pad material
  • Glass conveyor rollers and guides

Advantages

  • Extremely wear resistant
  • Low porosity prevents oil absorption
  • Low thermal conductivity
  • Capable of being machined or molded into exceptionally high tolerance parts

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.848 g/cc
Water Absorption 0.10 %after 24 hours at 23°C
 0.15 %after 24 hours at 50°C
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 88.0 MPa
Compressive Strength 172 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.830 W/m-K
Maximum Service Temperature, Air 315 °CContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek F-51 Dense Machinable Board
Overview of materials for Vinyl Ester Sheet Molding Compound
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Valcor® G Pre-Cast Shapes

PPYRO153 / 58408

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.