MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-150 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: This compound is inteded for use in medical and healthcare applications including high clarity tubing.

Uses: Medical/Healthcare Applications; Pharmaceuticals

Agency Ratings: ISO 10993 Part 5

Processing Method: Extrusion; Injection Molding

Forms: Pellets

Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Linear Mold Shrinkage 0.033 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.021 in/inASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52
@Time 5.00 sec
ASTM D2240
 54
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1150 psiASTM D412
Tensile Stress at Strain 350 psi
@Strain 100 %
ASTM D412
 430 psi
@Strain 200 %
ASTM D412
 520 psi
@Strain 300 %
ASTM D412
Elongation at Break 700 %ASTM D412
Tear Strength 41.2 kN/mASTM D624
Compression Set 18 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 95 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 185 °FContinuous; SAE j2236
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 320 °F
Middle Barrel Temperature 320 - 360 °F
Front Barrel Temperature 340 - 380 °F
Nozzle Temperature 380 - 420 °F
Zone 1 280 - 300 °F
Zone 2 300 - 320 °F
Zone 3 320 - 360 °F
Zone 5 340 - 380 °F
Die Temperature 360 - 400 °F
Melt Temperature 380 - 420 °FProcessing Temperature
Mold Temperature 70.0 - 100 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer

PTEKNO707 / 128885

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.