System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Nilit FRIANYL B63 V0 Nylon 6.6 for injection molding
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced, Flame Retardant
Material Notes:
Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.20
g/cc
ISO 1183
Water Absorption
2.0 - 3.0 %
ISO 62
Water Absorption at Saturation
7.0 - 8.0 %
ISO 62
Viscosity Measurement
145
Viscosity index; ISO 307
Linear Mold Shrinkage
0.012
-
0.025
cm/cm
FRISETTA Test Method
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
135
MPa
ISO 2039-1
Tensile Strength at Break
60.0
MPa
ISO 527
Elongation at Break
3.0 %
ISO 527
Tensile Modulus
3.50
GPa
ISO 527
Flexural Strength
90.0
MPa
ISO 178
Flexural Modulus
3.30
GPa
ISO 178
Charpy Impact Unnotched
3.00
J/cm²
DIN 53453
NB
ISO 179/1eU
2.00
J/cm²
@Temperature -40.0 °C
DIN 53453
Charpy Impact, Notched
0.500
J/cm²
ISO 179/1eA
0.500
J/cm²
DIN 53453
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
IEC 93
Dissipation Factor
0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index
600
V
CTI 100; IEC 112
600
V
CTI-M 100; IEC 112
Thermal Properties
Original Value
Comments
Melting Point
221
°C
ISO 3146 DSC
Maximum Service Temperature, Air
125
°C
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi)
185
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
85.0
°C
ISO 75
Flammability, UL94
V-0
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Celanese Nilit FRIANYL B63 GV25 Nylon 6 for injection molding, 25% glass fiber reinforced
Celanese Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Vanadium (II) Oxide, VO
Celanese Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding
PFRI176 / 39097
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.