MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Elvamide® 8061 PA6/66/610
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Polyamide Multipolymer

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccDAM; ASTM D 4052
Water Absorption 3.1 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 51.0 MPaDAM; ASTM D 638
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 °C10°C/min; DAM; ISO 11357-1/-3
 
Descriptive Properties
ISO designationISO 16396-PA6/66/610,,G1,,
Part Marking Code>PA6/66/610<ISO 11469
PolymerPA*
Resin IdentificationPA6/66/610ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 103FHSA NC010 PA66
Celanese Zytel® 151L NC010 PA612
Celanese Zytel® 77G33HS1L NC010 Nylon 612
Celanese Zytel® 101 NC010 PA66
EMS-Grivory Grilamid® XE 3959 black 9992 PA610

PDSX5166 / 197806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.