EVOLV3D™ LC 3335 Liquid Silicone Rubber is a 1:1 mix LSR designed for Liquid Additive Manufacturing (LAM) 3D printing. It combines the performance benefits of silicone rubber with the design and processing advantages of additive manufacturing. Product applications: - Preparation of silicone rubber prototypes with properties that are comparable to injection-molded components
- Low-volume or highly customized manufacturing of complex parts
- New design options in automotive, consumer care, cookware, lighting and other applications where traditional LSRs are used
Key Features:- Low viscosity
- Unique rheology
- Allows part design flexibility
- Enables achievement of mechanical properties closely matching those of molded LSR
- Direct transfer into high-volume injection-molding processes
- High-performance silicone elastomer parts – customized and/or new designs
Information provided by Dow |
 Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |