MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.

Main Application : Injection Moulding

Special Features : Combining hardness with excellent mechanical properties.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
Hardness, Shore D 49ISO 868
Tensile Strength, Yield 5801 psiISO 527-2/5A/500
Elongation at Break 515 %ISO 527-2/5A/500
50% Modulus 0.00900 GPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 1.74 ksi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 3.625 ksi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 880 pliISO 34-1B
Abrasion 20loss (mm³); ISO 306
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 121 °CISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 °C
Nozzle Temperature 210 °C
Zone 1 195 °C
Zone 2 200 °C
Zone 3 210 °C
Zone 4 210 °C
Dry Time 3.00 hour
@Temperature 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

PMES33 / 88410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.