MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Zelux® M Machine Grade Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Zelux® M is a machine grade polycarbonate (PC). This product is a transparent engineering thermoplastic with excellent dimensional stability, strength, and rigidity, along with service temperatures up to 250°F. This material has good insulating properties and is flame resistant. Zelux® M is also easy to fabricate, paint, and glue.

Industry: Aerospace; Engineering; Life Sciences; Semiconductor and ESD

Colors Available: Natural

Attributes: Dielectric Properties; Biocompatibility; Impact Resistance; Food Contact; Dimensional Stability

Shapes: Compression Sheet; Extruded Sheet; Extruded Rod

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9800 psiASTM D638
Tensile Strength, Yield 8900 psiASTM D638
Elongation at Break 135 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
Tensile Modulus 2.31 GPaASTM D638
Flexural Yield Strength 14000 psiASTM D790
Flexural Modulus 340000 psiASTM D790
Izod Impact, Notched 17.0 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10200 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 255 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Zelux® W Window Grade Polycarbonate
Covestro Makrolon® 3103 Polycarbonate
Techmer ES Elastoblend® PC IM
Westlake Plastics Zelux® 30% GF Polycarbonate
Westlake Plastics Zelux® 40% GF Polycarbonate

PWEST010 / 72714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.