MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® C 13031 XAS Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials.

Specific Notes for this Grade: Ideal property profile for sanitary applications. A new combination of stabilizers improves resistance to highly active acidic cleaning agents

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³10x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 1183
Melt Flow 17.04 g/10 min
@Load 2.16 kg,
Temperature 190 °C
17.04 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Calculated from Volume flow Rate: 12 cm3/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Elongation at Break 30 %30 %multi-purpose specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Elongation at Yield 11 %11 %multi-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Tensile Modulus 2.90 GPa421 ksimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 1 mm/min
Charpy Impact Unnotched 15.0 J/cm²
@Thickness 4.00 mm,
Temperature 23.0 °C
71.4 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
 0.800 J/cm²
@Thickness 4.00 mm,
Temperature 23.0 °C
3.81 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 13031 XF 50/5339 Acetal Copolymer
Celanese Hostaform® C 13021 XAP Acetal Copolymer
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
PTS POM-25 Acetal Copolymer

PHCX49 / 46079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.