MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring the TPE to be in direct contact with food. New Product. Commercial specifications have not been established. - Adhesion to Polypropylene, Low Density Polyethylene - Direct Food Contact - Enhanced Flow Properties - Excellent Colorability

Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Dynalloy™ OBC 8100-N75. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 175 to 800 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 3 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D792
Viscosity  28100 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
28100 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 120000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
120000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.0060 - 0.013 cm/cm0.0060 - 0.013 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.013 cm/cm0.0060 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 717110 sec; ASTM D2240
Tensile Strength at Break 5.63 MPa
@Temperature 23.0 °C
817 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain  3.56 MPa
@Strain 100 %,
Temperature 23.0 °C
516 psi
@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
 4.27 MPa
@Strain 300 %,
Temperature 23.0 °C
619 psi
@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 690 %
@Temperature 23.0 °C
690 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 36.4 kN/m208 pliASTM D624
Compression Set 30 %
@Temperature 23.0 °C,
Time 79200 sec
30 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 188 °C320 - 370 °F
Middle Barrel Temperature 177 - 193 °C351 - 379 °F
Front Barrel Temperature 182 - 210 °C360 - 410 °F
Nozzle Temperature 193 - 216 °C379 - 421 °F
Mold Temperature 15.6 - 26.7 °C60.1 - 80.1 °F
Back Pressure 0.000 - 0.689 MPa0.000 - 99.9 psi
Screw Speed 25 - 100 rpm25 - 100 rpm
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.2600
 
Descriptive Properties
Agency RatingsBfR Food Contact, Unspecified Rating
 EU 2002/72/EC
AppearanceNatural Color
FeaturesFood Contact Acceptable
 Good Colorability
 Good Flow
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesHousehold Goods
 Kitchenware
 Non-specific Food Applications
 Overmolding
 Soft Touch Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 6320 Magnesium Ionomer
Dow Engage® 8180 Polyolefin Elastomer
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
Avient Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE)
Avient Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)

PH0POL1198 / 145767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.