MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Varcum 29733 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29733 is a two-step, phenoxy modified, pulverized phenolic resin.

APPLICATION: Durez 29733 is recommended for the production of foundry snagging wheels.

FEATURES:

  • Provides significantly higher bursting speeds leading to greater metal removal rates.
  • Offers more durability and flexibility than wheels made with unmodified phenolic resins.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 200 MeshScreen %: < 8.0; DCT 4007A
 
Descriptive Properties
Hexa0.13DCT 4019A
Inclined Plate Flow20[mm]; DCT 4009A; hot; at 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 3509 Phenolic, Granular, Injection Molded
SCG Chemicals EL-Pro™ P851JO Polypropylene Injection Molding
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 GF Paper Phenolic
Sumitomo Bakelite Plyophen 43575 Phenolic Resin

PSUMIT731 / 194536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.