MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrocast AR FINE Castable Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall castings, or cast shapes with less than one inch cross section thickness. Parts cast form Pyrocast AR Fine are heat-treated as part of the manufacturing process to remove free and combined water.

Applications

  • Thimbles
  • Hot-top table sections
  • Transfer and stub troughs
  • Launder linings
  • Filter boxes
  • Sheet ingot spouts
  • Control pins
  • Furnace tubes

Advantages

  • Dimensionally stable
  • Thermal shock resistant
  • Easily cleaned
  • Extremely durable
  • Smooth cast surface
  • Preheating unnecessary
  • Non-wetting

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.86 - 1.89 g/cc0.0672 - 0.0683 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00850 GPa
@Temperature 725 °C
1.23 ksi
@Temperature 1340 °F
 0.00615 GPa
@Treatment Temp. 650 °C
0.892 ksi
@Treatment Temp. 1200 °F
Compressive Strength 43.2 MPa6270 psicured at 650°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.320 µm/m-°C
@Temperature 650 °C
0.178 µin/in-°F
@Temperature 1200 °F
Thermal Conductivity  0.590 W/m-K
@Temperature 400 °C
4.09 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.710 W/m-K
@Temperature 550 °C
4.93 BTU-in/hr-ft²-°F
@Temperature 1020 °F
 0.820 W/m-K
@Temperature 700 °C
5.69 BTU-in/hr-ft²-°F
@Temperature 1290 °F
Shrinkage 0.40 %
@Temperature 815 °C
0.40 %
@Temperature 1500 °F
Linear
 
Processing PropertiesMetricEnglishComments
Processing Temperature 760 °C1400 °FException: Not recommended for use in continuous casting applications.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrotek PTB 2200 Structural Board
Pyrotek Pyrocast 220HT Refractory Castable
Pyrotek Pyrocast AR Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable

CPYRO175 / 1892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.