MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American White Ash Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Least easy to work with hand tools. Excellent shaping, very good planing, very good steam bending. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Fraxinus americana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.550 g/ccOven Dry Weight/Unseasoned Volume
 48.0 lb/ft³Unseasoned*
Cell Length 1.20 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4000 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4400 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 5900 NSide
Tensile Strength, Ultimate 6.50 MPaPerpendicular to Grain
 620 psiPerpendicular to Grain*
Modulus of Rupture 0.106 GPaIn Bending
 9.10 ksiStatic Bending*
Flexural Yield Strength 61.4 MPaBending stress at proportional limit
 4900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 12.0 - 12.4 GPaIn Bending
 1350 ksiStatic Bending*
Compressive Strength 8.00 MPaPerpendicular to Grain
 51.0 MPaParallel to Grain
 800 psiPerpendicular to Grain*
 3230 psiParallel to Grain*
 3800 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.051µTL, 12% Moisture Content
 0.059µRL, 12% Moisture Content
 0.36µTR, 12% Moisture Content
 0.371µLR, 12% Moisture Content
 0.44µLT, 12% Moisture Content
 0.684µRT, 12% Moisture Content
Shear Strength 13.4 MPaOrientation Unknown
 1260 psiParallel to Grain*
Impact 5.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 11700psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 1.03 in-lb/in³Static Bending*
Work to Maximum Load 13.4 in-lb/in³Static Bending*
Cleavage 58.0 kN/mRadial surface of failure, Unseasoned*
 61.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 µm/m-°C
@Temperature 20.0 °C
Axial. Typical value for Ash.
Thermal Conductivity 0.980 BTU-in/hr-ft²-°FOven Dry
 1.20 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.9 %Radial; Unseasoned to Oven Dry*
 7.9 %Tangential; Unseasoned to Oven Dry*
 13.2 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5086-H116; 5086-H32
Aluminum 5052-H32
Aluminum 5083-H116; 5083-H321
American Ash Wood
European Ash Wood

PTSAM / 71296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.