  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® V/T-2UV (06022020) Curable Polyethylene System
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® V/T-2UV is a low density flame-retardant XLPE system curable by moisture and consists of a silane grafted base compound A-3001 and a catalyst masterbatch CAT-083FR-UV. Mixed and extruded in the proper proportions (50/50), the two components result in a material that is curable by exposure to hot water. PEXIDAN® V/T-2UV is halogenated but is RoHS-compliant. Insulation made with this system may be marked SUNRES or ‘SR’ in all colors and in all sizes per UL44, UL4703 and CSA C22.2 #38. This product is also CSA-listed for RW90, RWU90, RPV90 RPVU90 and CIC, ‘SR’ and -40C rated.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Deformation 9.0 %UL 1581 / UL 2556
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1930 psiUL 1581 / UL 2556
 1950 psiWeather-o-meter testing - 720 hr. exposure - SUNRES; UL 1581 / UL 2556
 1790 psi
@Temperature 23.0 °C
30 day gasoline; UL 1581 / UL 2556
 1815 psi
@Temperature 75.0 °C
60 day oil; UL 1581 / UL 2556
 1950 psi
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Elongation at Break 275 %Weather-o-meter testing - 720 hr. exposure - SUNRES; UL 1581 / UL 2556
 300 %UL 1581 / UL 2556
 290 %
@Temperature 75.0 °C
60 day oil; UL 1581 / UL 2556
 320 %
@Temperature 23.0 °C
30 day gasoline; UL 1581 / UL 2556
 45 %
@Temperature 150 °C,
Time 900 sec
Hot, Elongation under 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 300 %
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Crush Resistance 1360 lb (mass)UL 1581 / UL 2556
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Temperature 90.0 °C
UL 1581 / UL 2556
Dielectric Breakdown 21 VAfter glancing impact; UL 1581 / UL 2556
 30000 VUL 1581 / UL 2556
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -60.0 °CLow Temperature Brittleness Point; ASTM D746
Oxygen Index 27 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 310 - 340 °Fbarrel zones
Die Temperature 365 °F
Head Temperature 365 °F
 
Descriptive Properties
Degree of Crosslinking60%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO053 / 249420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.