MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum friction resistance.

Special Properties:
Extremely high conductivity
Voltage dissipation on the surface in less than 0.1s
Reduction in drive power with no reduction in performance
Minimal and constant sliding friction coefficient even in continuous operation
Self-lubricating
Approved for use in the food industry (EU and/or FDA)

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PE-UHMW
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.930 g/ccISO 1183
Molecular Weight 9.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60DIN 53505
Ball Indentation Hardness 30.0 MPa
Tensile Strength 20.0 MPaISO 527
Elongation at Break 255 %ISO 527
Modulus of Elasticity 0.700 GPa
Charpy Impact, Notched >= 150 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.060 - 0.10
Sand Slurry 80value in %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1000 ohm-cmIEC 60093
Surface Resistance <= 1.00e+9 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.400 W/m-KISO 52612
Maximum Service Temperature, Air 90.0 °CShort Term
 80.0 °C
@Time 1.80e+7 sec
Minimum Service Temperature, Air -200 °C
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
Hippe PE 500 Polyethylene
Asahi Kasei Tenac® FA405 Acetal Homopolymer, Low Friction Grade
Polyram RamTal PM1509 Acetal, Low Friction
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene

PMURT910 / 156557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.