MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 0.028" (0.7112 mm) Flexible Heater Silicone with Fiberglass Substrate (55586W028)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Silicone

Material Notes: 0.004 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.028 in + 0.003, -0.000 (0.71 mm + 0.08, -0.00). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: White. Weight: 1305 g/m² ± 102 (38.5 oz./yd.² ± 3.0). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours.

Information provided by the manufacturer, Arlon Silicone Technologies Division.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 5040 - 50
Tensile Strength, Ultimate 5.58 - 6.82 MPa809 - 989 psi
Elongation at Break 540 - 660 %540 - 660 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.75 kV/mm>= 400.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °Fper UL Card E54153
 232 °C450 °F
Minimum Service Temperature, Air -56.6 °C-69.9 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 176.6 °C349.9 °Fcuring temp., at 0.345 MPa (50 psi)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASB80 / 24714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.