MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements.

Regulatory Status: M6010SB meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows for, among other things, the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Certain limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Certain recommendations for processing M6010SB can only be made when the processing conditions, equipment and end use are provided; however, Equistar recommends that samples be produced and that users conduct their own testing in order to make their own independent determination that M6010SB is suitable and safe for their intended use and applications.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccASTM D1505
Thickness 1.25 mil
Melt Flow 1.1 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 4000 psiASTM D882
Film Tensile Strength at Yield, TD 4800 psiASTM D882
Film Elongation at Break, MD 700 %ASTM D882
Film Elongation at Break, TD 400 %ASTM D882
Secant Modulus, MD 0.986 GPaASTM E111
Secant Modulus, TD 1.38 GPaASTM E111
Elmendorf Tear Strength MD 20 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Film Tensile Strength at Break, MD 8800 psiASTM D882
Film Tensile Strength at Break, TD 3600 psiASTM D882
 
Processing PropertiesOriginal ValueComments
Melt Temperature 390 - 410 °F
Die Opening 0.1524 cm
Blow-up Ratio (BUR) 2.2
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M5010 High Density Polyethylene, MMW Film Grade
LyondellBasell Alathon® L4907 High Density Polyethylene
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
Ineos TUB 172 HDPE
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade

PEQU0783 / 104139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.