MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade; Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Description: Pluris4303 is a Braskem Quaterpolymer produced with Spherilene technology. This grade show unique properties, such as high stiffness associated with toughness. In addition to good processability, also shows a very good bubble stability and very low gel content.

Applications: Thin films and automatic packaging which require higher stiffness: textile products, toilet paper and others.

Additive: Antiblocking medium; Slip medium

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccASTM D792
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 920 %ASTM D882
Film Elongation at Break, TD 1450 %ASTM D882
Elmendorf Tear Strength MD 50 gASTM D1922
Elmendorf Tear Strength TD 300 gASTM D1922
Film Tensile Strength at Break, MD 32.0 MPaASTM D882
Film Tensile Strength at Break, TD 33.0 MPaASTM D882
1% Secant Modulus, MD 310 MPaASTM D882
1% Secant Modulus, TD 400 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 43 %ASTM D1003
Gloss 45 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 170 °CProfile

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem HF2007 Blown Film Extrusion Linear Low Density Polyethylene
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene
Braskem LF1020/21AF Blown Film Extrusion Linear Low Density Polyethylene

PBRASK2104 / 199985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.