MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos R55C-00 Clarified Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling capabilities, excellent clarity, fast cycle times and good stiffness-to-impact properties balance. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520. Preliminary properties listed below could later be subject to minor change.
    Applications:
  • Thin wall injection molding (TWIM) of multi-cavity parts
  • Stadium cups and containers
  • Audio/video media rigid packaging formats
  • Consumer products and housewares
    Benefits:
  • High flow rate for easier mold filling
  • High clarity in thin-walled parts
  • Fast cycling
  • Low bloom and good static charge dissipation
  • Very good impact resistance

    Information provided by Ineos Olefins & Polymers USA

Key Words: Excellent clarity, fast cycle times and good stiffness-to-impact properties balance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 55 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 84.4ASTM D785
Tensile Strength, Yield 4250 psiASTM D638
Flexural Modulus 155.6 ksiASTM D790A
Izod Impact, Notched 0.910 ft-lb/in1/8" (3mm) notched bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 84.7 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 17.3 %
@Thickness 1.27 mm
plaque, Diffuse Transmittance; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H02C-00 Polypropylene Homopolymer
Ineos H11G-01 Polypropylene Homopolymer
Ineos H12E-00 Polypropylene Homopolymer, Antistatic
Ineos H12G-00 Polypropylene Homopolymer
Ineos H12G-01 Polypropylene Homopolymer

PINEOS916 / 130375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.