MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polycarbonate, Glass + PTFE Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass + PTFE Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.28 - 1.61 g/cc0.0462 - 0.0582 lb/in³Average value: 1.43 g/cc Grade Count:98
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 20.3 % Grade Count:44
Water Absorption 0.0170 - 0.250 %0.0170 - 0.250 %Average value: 0.101 % Grade Count:54
Additive Loading 15.0 - 30.0 %15.0 - 30.0 %Average value: 22.1 % Grade Count:7
Linear Mold Shrinkage 0.000500 - 0.00800 cm/cm0.000500 - 0.00800 in/inAverage value: 0.00302 cm/cm Grade Count:95
Linear Mold Shrinkage, Transverse 0.00400 - 0.00700 cm/cm0.00400 - 0.00700 in/inAverage value: 0.00529 cm/cm Grade Count:7
Melt Flow 3.00 - 15.0 g/10 min3.00 - 15.0 g/10 minAverage value: 8.62 g/10 min Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 90.0 - 95.090.0 - 95.0Average value: 92.3 Grade Count:3
Hardness, Rockwell R 114 - 120114 - 120Average value: 117 Grade Count:29
Tensile Strength, Ultimate 9.81 - 124 MPa1420 - 18000 psiAverage value: 82.6 MPa Grade Count:91
Tensile Strength, Yield 1.47 - 121 MPa213 - 17500 psiAverage value: 75.0 MPa Grade Count:16
Elongation at Break 1.00 - 120 %1.00 - 120 %Average value: 5.46 % Grade Count:86
Elongation at Yield 2.60 - 7.00 %2.60 - 7.00 %Average value: 4.00 % Grade Count:6
Modulus of Elasticity 2.41 - 13.8 GPa350 - 2000 ksiAverage value: 6.11 GPa Grade Count:76
Flexural Yield Strength 39.3 - 193 MPa5700 - 28000 psiAverage value: 132 MPa Grade Count:96
Flexural Modulus 2.28 - 10.7 GPa331 - 1550 ksiAverage value: 5.55 GPa Grade Count:94
Compressive Yield Strength 72.4 - 110 MPa10500 - 16000 psiAverage value: 92.2 MPa Grade Count:8
Izod Impact, Notched 0.320 - 12.3 J/cm0.600 - 23.0 ft-lb/inAverage value: 1.70 J/cm Grade Count:96
Izod Impact, Unnotched 0.801 - 16.0 J/cm1.50 - 30.0 ft-lb/inAverage value: 7.95 J/cm Grade Count:68
Izod Impact, Notched (ISO) 9.50 - 17.9 kJ/m²4.52 - 8.52 ft-lb/in²Average value: 12.8 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) 34.4 - 58.1 kJ/m²16.4 - 27.6 ft-lb/in²Average value: 43.5 kJ/m² Grade Count:5
Charpy Impact Unnotched 2.20 - 2.20 J/cm²
@Temperature -30.0 - -30.0 °C
10.5 - 10.5 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.20 J/cm² Grade Count:1
Falling Dart Impact 11.6 - 18.4 J8.56 - 13.6 ft-lbAverage value: 15.9 J Grade Count:6
Instrumented Impact Total Energy 3.45 - 7.05 J2.54 - 5.20 ft-lbAverage value: 5.01 J Grade Count:5
Coefficient of Friction 0.200 - 0.5500.200 - 0.550Average value: 0.410 Grade Count:4
Coefficient of Friction, Static 0.180 - 0.4800.180 - 0.480Average value: 0.332 Grade Count:4
K (wear) Factor 15.0 - 254 x 10-8 mm³/N-M7.45 - 126 x 10-10 in³-min/ft-lb-hrAverage value: 108 x 10-8 mm³/N-M Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 1.00e+16 ohm-cm1000 - 1.00e+16 ohm-cmAverage value: 7.18e+15 ohm-cm Grade Count:56
Surface Resistance 1000 - 1.00e+16 ohm1000 - 1.00e+16 ohmAverage value: 1.60e+15 ohm Grade Count:12
Dielectric Constant 3.20 - 3.403.20 - 3.40Average value: 3.34 Grade Count:5
Dielectric Strength 17.7 - 18.1 kV/mm450 - 460 kV/inAverage value: 17.9 kV/mm Grade Count:5
Dissipation Factor 0.00700 - 0.01000.00700 - 0.0100Average value: 0.00780 Grade Count:5
Arc Resistance 120 sec120 secAverage value: 120 sec Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 - 58.0 µm/m-°C13.0 - 32.2 µin/in-°FAverage value: 32.3 µm/m-°C Grade Count:17
Thermal Conductivity 0.202 - 0.317 W/m-K1.40 - 2.20 BTU-in/hr-ft²-°FAverage value: 0.272 W/m-K Grade Count:9
Maximum Service Temperature, Air 130 - 150 °C266 - 302 °FAverage value: 141 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 136 - 182 °C277 - 360 °FAverage value: 145 °C Grade Count:50
Deflection Temperature at 1.8 MPa (264 psi) 121 - 149 °C250 - 300 °FAverage value: 140 °C Grade Count:76
Vicat Softening Point 150 - 160 °C302 - 320 °FAverage value: 157 °C Grade Count:4
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:69
 
Processing PropertiesMetricEnglishComments
Processing Temperature 249 - 299 °C480 - 570 °FAverage value: 272 °C Grade Count:22
Melt Temperature 221 - 338 °C430 - 640 °FAverage value: 302 °C Grade Count:62
Mold Temperature 65.6 - 121 °C150 - 250 °FAverage value: 96.5 °C Grade Count:82
Drying Temperature 110 - 130 °C230 - 266 °FAverage value: 121 °C Grade Count:59
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:44
Dew Point -28.9 °C-20.0 °FAverage value: -28.9 °C Grade Count:36
Injection Pressure 41.4 - 138 MPa6000 - 20000 psiAverage value: 86.8 MPa Grade Count:58
Vent Depth 0.00127 - 0.00760 cm0.000500 - 0.00299 inAverage value: 0.00253 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, 30% Glass Filled
Overview of materials for Polycarbonate, Carbon + PTFE Filled
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
Overview of materials for Polycarbonate, Stainless Steel Fiber

O3153 / 78144

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.