MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Atom Adhesives AA-BOND F156 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opaque adhesive for light sensitive components is required. AA-BOND F156 is two parts smooth paste formulation is easy to use, develops strong bonds to itself and to most materials. AA-BOND F156 exhibits low shrinkage during cure, has excellent dimensional stability over a wide temperature range.

Appearance: Black, Opaque

Cure Type: Heat cure or Room Temperature

Benefits:

  • Easy to use
  • Good low-temperature structural, physical and electrical properties
  • It’s resistant to water, weater, gases, salts, mild acids, alkalis, and many organic and inorganic compounds
Mix Ratio by weight: 100:12/Resin:Hardener

Substrates: Glass and glass fabrics, ceramics, leather, metals and many plastics

Typical Application: High quality photographic industry bonding, laminating, production and repair applications where a room-temperature cure optically opaque adhesive for light sensitive components is required

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/ccuncured
Solids Content 100 %reactive, uncured
Viscosity 50000 cPAfter mixing, uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90cured
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.3
@Frequency 1000 Hz
Dielectric Strength 390 kV/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.9 µm/m-°C
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 95.0 °Ccured
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30.0 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PATOM022 / 172337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.