MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsui MILEX™ RN-2830MR Acrylic Rubber Modified Phenolic Resin
Categories: Polymer; Thermoset; Phenolic; Phenolic/Rubber; Molded

Material Notes: The MILEX™ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad and clutch facing disc friction materials. The advantage of incorporating the MILEX material into a brake design is that the material provides a non-abrasive, vibratory free surface finish, which is very important in the performance of the brake system. Additionally, its superior performance at elevated temperatures and excellent moldability aids in brake noise reduction.

The RN series are novolak type phenolic resins modified by special elastomers. This series consists of a grouping of acrylic rubber modified resin in addition to the RS-2210MB grade, a silicon rubber modified resin. This series is recognized worldwide by the automotive industry for its thermal shock and chemical resistant properties. In addition, this particular series possesses anti-brake noise and vibratory qualities in brake pad applications. Some of the most demanding electrical applications choose phenolic resin due to the material's high dielectric strength, superior insulation resistance and high temperature resistance. Typical applications include use as an Epoxy Resin hardener for electronic materials such as encapsulation for I.C., an adhesive with elastomers and to improve the high heat resistance of thermoplastics.

Applications:

  • Automotive friction materials (brake pads, clutch facing discs, etc)
  • Epoxy resin hardener for electronic materials
  • Additive to improve heat resistance of thermoplastics
  • Adhesives, especially with elastomers, to bond to metal

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 - 105 °CSoftening point
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °CPress Cure, 8-10 minutes
 180 °CPost cure, 5 hours
Gel Time 0.583 - 1.58 min
 
Descriptive Properties
Cracking Resistance45=Excellent
Curing Rate51=Slow, 5=Fast
Flow15-40 m/m
Hardness31=Hard, 5=Soft
Heat Resistance11-5 (5-Excellent)
Kind of RubberAcrylic
Rubber Content30 phr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMIT058 / 53239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.