MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow VERSIFY™ 3401 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: VERSIFY™ 3401 Elastomer is a resin with a medium melt flow rate suitable for a wide variety of applications and fabrication processes. Including cast film, extrusion and injection molding. It is an excellent resin for stretch films and soft films, and is an excellent choice for PP modification, giving consistent performance in hot and cold conditions

Main Characteristics:

  • White Pellet
  • Free flowing
  • Medium flow
  • Excellent elasticity
  • Excellent compatibility with PP
Applications:
  • Stretch film
  • Overmolding
  • Soft film
  • PP modification
Complies with
  • EU, No 10/2011
  • US FDA FCN 909
Consult the regulations for complete details.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.863 g/ccASTM D792
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Crystallinity 14 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 72
@Time 10.0 sec
Compression Molded; ASTM D2240
Hardness, Shore D 22
@Time 10.0 sec
Compression Molded; ASTM D2240
Tensile Strength at Break 6.80 MPaCompression Molded; ASTM D638
Elongation at Break 600 %50 mm/min, Compression Molded; ASTM D638
Flexural Modulus, 1% Secant 22.7 MPaCompression Molded; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 55.0 °CDSC
Vicat Softening Point <= 20.0 °CASTM D1525
Glass Transition Temp, Tg -29.8 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 3.2 %
@Thickness 2.00 mm
Injection Molded; ASTM D1003
Gloss 63 %
@Thickness 1.00 mm
20°, Compression Molded, Gardner; ASTM D523
 112 %
@Thickness 1.00 mm
60°, Compression Molded, Gardner; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VERSIFY™ 3200 Elastomer
Dow VERSIFY™ 2200 Plastomer
Dow VERSIFY™ 3300 Elastomer
Dow VERSIFY™ 4200 Plastomer
Dow VERSIFY™ 2000 Plastomer

PDOW2039 / 183686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.