MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zenite® 5145L BK010 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: Zenite® 5145L BK010 is a 45% glass reinforced, lubricated liquid crystal polymer resin with excellent toughness and a heat deflection temperature of 290°C.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.76 g/ccASTM D 792
Density 1.75 g/ccISO 1183
Filler Content 45 %
Linear Mold Shrinkage, Flow 0.00090 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPaISO 527
Tensile Strength, Ultimate 130 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 3.1 %ISO 527
 3.3 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 15000 MPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 160 MPa
@Temperature 23.0 °C
ASTM D 790
 190 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 11000 MPa
@Temperature 23.0 °C
ISO 178
 13000 MPa
@Temperature 23.0 °C
ASTM D 790
Izod Impact, Notched 2.50 J/cm
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 600 J/m
@Temperature 23.0 °C
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D 257
Surface Resistance 1.00e+15 ohmASTM D 257
Dielectric Constant 3.4
@Frequency 1000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.9
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D 150
 4.4
@Frequency 100000 Hz,
Temperature 23.0 °C
ASTM D 150
 4.5
@Frequency 10000 Hz,
Temperature 23.0 °C
ASTM D 150
 4.7
@Frequency 1e+9 Hz,
Temperature 23.0 °C
2.0mm; ASTM D 2520 B
 4.8
@Frequency 1e+10 Hz,
Temperature 23.0 °C
2.0mm; ASTM D 2520 B
 5.0
@Frequency 2.00e+10 Hz,
Temperature 23.0 °C
2.0mm; ASTM D 2520 B
Dielectric Strength 22.0 kV/mm
@Temperature 23.0 °C
500 V/s, Short Time; ASTM D 149
 24.0 kV/mm
@Thickness 2.00 mm,
Temperature 150 °C
IEC 60243-1
 24.0 kV/mm
@Thickness 2.00 mm,
Temperature 200 °C
IEC 60243-1
 27.0 kV/mm
@Thickness 2.00 mm,
Temperature 100 °C
IEC 60243-1
 35.0 kV/mm
@Thickness 1.00 mm,
Temperature 200 °C
IEC 60243-1
 40.0 kV/mm
@Thickness 1.00 mm,
Temperature 150 °C
IEC 60243-1
 40.0 kV/mm
@Thickness 1.00 mm,
Temperature 100 °C
IEC 60243-1
 45.0 kV/mm
@Thickness 1.00 mm,
Temperature 23.0 °C
IEC 60243-1
Dissipation Factor 0.014
@Frequency 10000 Hz
ASTM D 150
 0.017
@Frequency 1000 Hz
ASTM D 150
 0.018
@Frequency 100000 Hz
ASTM D 150
 0.018
@Frequency 1e+6 Hz
ASTM D 150
 0.0060
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D2520 B
 0.0060
@Thickness 2.00 mm,
Frequency 1e+10 Hz
ASTM D2520 B
 0.0080
@Thickness 2.00 mm,
Frequency 2.00e+10 Hz
ASTM D2520 B
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear -1.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 0.000 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 7.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 52.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 2mm
 52.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 4mm
 77.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 2mm
 80.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 4mm
 60.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 60.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 80.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 80.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 95.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 100 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
Melting Point 319 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 275 °CASTM D 648
 290 °CISO 75-1/-2 1993/N2
UL RTI, Electrical 130 °C
@Thickness 0.800 mm
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.800 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.800 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 0.800 mm
UL94
 V-0
@Thickness 3.00 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
Glow Wire Ignition Temperature 800 °C
@Thickness 2.00 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 335 °COptimum
 325 - 345 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericLCP
Part Marking Code>LCP-GF45<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Celanese VECTRA V143XL LCP, 42% Glass Reinforced
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Celanese VECTRA E471i LCP, 35% Specialty
Celanese VECTRA E488i LCP, Specialty

PDTA7772 / 89569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.