MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of good extrudability and electrical properties. LR4201S is natural in color.

LR4201S has been specifically developed for medium and high voltage power cables. Because it is a Superclean material, LR4201S is suitable for use in high voltage cables rated up to 161 kV.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccBase Resin; ASTM D1928/D 1505
ESCR 100% Igepal® >= 1000 hourASTM D1693
ESCR 10% Igepal® >= 1000 hourASTM D1693
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Base Resin; ISO 1133
Degree of Crosslinking 12 %ASTM D2765
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength, Yield >= 1980 psiHeat Aging (168 hrs at 136°C); ASTM D638
 2200 psiAt 20 in/min; ASTM D1238
Elongation at Break <= 75 %Hot Creep Test (150°C,29 psi); ICEA T-28-562
 400 %ASTM D638
Tensile Set 5.0 %Hot Creep Test (150°C,29 psi); ICEA-T-28-562
 360 %Retention; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 550 V/mil
@Thickness 1.30 mm
ASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables
Borealis Borlink™ LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0315 Polyethylene Compound, Crosslinkable, Semiconductive
Syensqo (Solvay Specialty Polymers) Polidan® EC/51 Polyethylene, Crosslinked (XLPE)

PBOREA191 / 27498

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.