MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NAECO® NAECOMET® D581F Silver Graphite Contact Material
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: For electrical contacts; reduced sticking, low friction.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.3 g/cc0.372 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 44 - 7244 - 7244 (annealed) - 72 (worked)
Tensile Strength, Ultimate 169 MPa24500 psiAnnealed
 252 MPa36500 psiWorked
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000169 ohm-cm0.00000169 ohm-cm(102% IACS)
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 980 °C<= 1800 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 %0.50 %
Silver, Ag 99.5 %99.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® NAECOMET® D58 Silver Graphite Contact Material
NAECO® NAECOMET® D158F Silver Graphite Contact Material
NAECO® NAECOMET® D1058 Silver Graphite Contact Material
NAECO® NAECOMET® D582F Silver Graphite Contact Material
NAECO® NAECOMET® D583F Silver Graphite Contact Material

NCMV825 / 192405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.