MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ArcelorMittal 300 BH Bake hardening steel, Cold rolled
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: uncoated (HC300B), electroglavanized (HC300B+ZE) and Extragal®/Galvannealed (HC300BD+Z)

Description: The composition and processing of these steels are designed to promote a significant increase in yield strength during low-temperature heat treatment, particularly paint curing. ArcelorMittal Bake hardening steels can thus achieve higher strength in the finished part while retaining good forming performance. The gain in yield strength through the "bake hardening" (BH) effect is generally greater than 40 MPa. Thanks to this BH effect, ArcelorMittal steels offer two advantages compared to conventional drawing quality steels:

  • Improved dent resistance in all finished parts in the case of low forming strains (hood, roof, doors and wings);
  • Substantial weight reduction potential at equivalent dent resistance (the decrease in thickness is offset by increased yield strength resulting from the heat treatment process).
Bake hardening steels thus offer a suitable response to automotive bodywork requirements. By providing an excellent drawability-dent resistance combination, they enhance vehicle weight reduction and aesthetics.

Applications: Steels in the BH range are designed for visible (door, hood, tailgate, front wing, roof) and structural (underbody, reinforcement, cross member, lining) parts

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 420 - 480 MPa
Tensile Strength, Yield 300 - 360 MPa
Elongation at Break >= 28 %L0=80 mm, th<3 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Iron, Fe >= 98.7 %as balance
Manganese, Mn <= 0.70 %
Silicon, Si <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061-T4; 6061-T451
ArcelorMittal HSLA 300 High strength low alloy steel for cold forming, Cold Rolled
ATI Allvac® VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
ArcelorMittal Usibor® 1500 Ultra high strength steel, Hot Rolled
ArcelorMittal H 360 Solid solution steel, Cold rolled

NARCE053 / 159961

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.