MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jushi E7 DR-386T Direct Roving - Polyester Composite
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: E7 DR-386T is recommended for reinforcement of unsaturated polyester, vinyl ester, and epoxy resins for weaving, pultrusion, and filament winding. High modulus glass coated with silane-based sizing. Excellent processing. Fast wet-out. Uses include windmill blades, marine, pipe, tubes, tanks, and pultruded structures.

Property data for E7DR17-2400-386T + polyester composites.

Information provided by Jushi Group Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium <= 0.10 %Fiber value; ISO 3344
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2590 MPaStrand Tensile; ASTM D2343
Modulus of Elasticity 88.2 GPa
Tenacity >= 0.450 N/texFiber breaking strength; ISO 3341
Shear Strength >= 54.8 MPaInterlaminar shear NOL ring, After 72 hour boil; ASTM D2344
 64.5 MPaInterlaminar shear NOL ring, Dry; ASTM D2344

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jushi E7 DR-386T Direct Roving - Epoxy Composite
Jushi E7 DR-380 Direct Roving - Epoxy Composite
Aluminum 6063-T6
BCC Products BC 8990 Polyurethane Elastomer
BCC Products BC 8870 Polyurethane Elastomer

PJUSHI992 / 183364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.