MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HGC-4-C Precious dental alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 16.7 - 18.1 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 150 - 200soft
 220 - 230hardened
Tensile Strength, Ultimate 530 - 580 MPasoft
Tensile Strength, Yield 550 - 650 MPahardened
 380 - 480 MPa
@Strain 0.2 %
soft
 470 - 600 MPa
@Strain 0.2 %
hardened
Elongation at Break 3.0 - 6.0 %hardened
 7.0 - 14 %soft
Modulus of Elasticity 102 - 113 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 - 16.8 µm/m-°C
@Temperature 25.0 - 600 °C
Melting Point 900 - 1260 °C
Solidus 900 °C
Liquidus 1260 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 0.00 - 5.0 %
Gold, Au 50 - 73 %
Indium, In <= 2.0 %
Iridium, Ir <= 0.10 %
Palladium, Pd <= 1.0 %
Platinum, Pt <= 1.9 %
Rhenium, Re <= 0.10 %
Silver, Ag 10 - 28 %
Zinc, Zn 12 - 14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
NAECO® NAECOMET® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
NAECO® NAECOMET® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
NAECO® NAECOMET® D158F Silver Graphite Contact Material
NAECO® NAECOMET® D355F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

MMEDIC37 / 12413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.