MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent resistance and dimensional stability of the finished garment. For technical applications, GRILTEX adhesive products are used to optimize the manufacturing process for the production of automotive interior components or parts for other applications. All values were determined on dried pellets.

Main Application System: Paste Dot, Powder Dot, Top Dot, Scatter Coating

Main Usage: Men's and Children's Wear, Women's Wear, Leisure and Sports Wear, Uniforms

Data provided by EMS-Griltech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 170000 cP
@Temperature 160 °C
2.16 kg load; ISO 1133
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 160 °C
cm3/10 min; ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 115 - 125 °CDSC
Maximum Service Temperature, Air <= 60.0 °CLaundering Resistance
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 - 150 °CGlue Line Temperature
Roll Temperature 45.0 - 55.0 °CTemperature of Engraved Rolls
 
Descriptive Properties
Dry Cleaning ResistanceVery Good
Steam ResistanceVery Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Arkema LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate

PGRIL319 / 43171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.