MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® TTX163 + MOCA, 95 A Polyurethane, TDI- PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccDESMODUR® TT163
 1.12 g/cc1.12 g/cc
 1.25 g/cc1.25 g/ccMOCA
Viscosity 400 cP400 cPDESMODUR® TT163
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595DIN 53505
 95
@Temperature 80.0 °C
95
@Temperature 176 °F
DIN 53505
 96
@Temperature -5.00 °C
96
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 50.0 MPa7250 psiDIN 53504
Tensile Stress at Strain 6.50 MPa
@Strain 10 %
943 psi
@Strain 10 %
DIN 53504
Elongation at Break 330 %330 %DIN 53504
100% Modulus 13.9 MPa
@Strain 100 %
2020 psi
@Strain 100 %
DIN 53504
200% Modulus 21.3 MPa
@Strain 200 %
3090 psi
@Strain 200 %
DIN 53504
300% Modulus 42.1 MPa
@Strain 300 %
6110 psi
@Strain 300 %
DIN 53504
Resilience 4343[%]; DIN 53512
Tear Strength 53.0 kN/m302 pliwith nick; ISO 34-1
 110 kN/m628 pliwithout nick; ISO 34-1
Abrasion 5050[mm3]; ISO 4649
Compression Set 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FDESMODUR® TT163
 120 °C248 °FMOCA
Mold Temperature 100 °C212 °F
Pot Life 5.00 min5.00 min
 
Descriptive Properties
AppearanceliquidDESMODUR® TT163
 solidMOCA
Content100Parts by weight of prepolymer
 19Parts by weight of MOCA
 6.1-6.5%NCO, DESMODUR® TT163

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® TT163 + BAYTEC® XL 2190, 58 D Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX174 + MOCA, 60 D Polyurethane, TDI- PTMEG
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTG528 + MOCA Polyurethane, TDI- Ether
Covestro DESMODUR® TTX131 + MOCA, 85 A Polyurethane, TDI- PTMEG

PCOVEST0653 / 202436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.