MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow HDPE 05862N High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 g/cc
Thickness 25.0 microns
Melt Flow 5.0 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 8.1.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 27.5 MPa
Film Tensile Strength at Yield, TD 28.3 MPa
Film Elongation at Break, MD 595 %
Film Elongation at Break, TD 650 %
Secant Modulus, MD 0.472 GPaFilm value
Secant Modulus, TD 0.572 GPaFilm value
Elmendorf Tear Strength MD 40 g
Elmendorf Tear Strength TD 118 g
Elmendorf Tear Strength, MD 1.60 g/micron
Elmendorf Tear Strength, TD 4.70 g/micron
Dart Drop 1.60 g/micron
Film Tensile Strength at Break, MD 35.6 MPa
Film Tensile Strength at Break, TD 28.0 MPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 130 °C
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %
Gloss 85 %45°
 
Processing PropertiesOriginal ValueComments
Processing Temperature 274 °CFilm extrusion temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow HDPE 25455N High Density Polyethylene
Dow DOWLEX™ IP-10262 High Density Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Dow DOWLEX™ IP-41 High Density Polyethylene
Dow HDPE 17450N High Density Polyethylene

PDW474 / 34543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.