MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® T80 Toluene Diisocyanate
Categories: Fluid

Material Notes: Description: Lupranate® T80 toluene diisocyanate (TDI) is an 80% - 20% mixture of the 2,4 and 2,6 isomers of toluene diisocyanate. This product is used in the preparation of polyurethane foams, prepolymers and elastomers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Vapor Pressure 0.0000133 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 12.0 °CFreezing Point
Boiling Point >= 120 °C
@Pressure 0.0000917 MPa
Flash Point 132 °C
 
Descriptive Properties
Acidity, as HCI<0.003%Type 1, as HCl, STI 8202
 0.007-0.009%Type 2, as HCl, STI 8202
Assay>99.5%Type 1, STI 8207
 >99.5%Type 2, STI 8207
Color<15APHA, Type 1, STI 8206
 <15APHA, Type 1, STI 8206
CompositionHydrolyzable Chlorine<0.007%, Type 1, STI 8203
 Hydrolyzable Chlorine0.008-0.012%, Type 2, STI 8203
Isomer Ratio19-21%-2,6, Type 1, STI 8207
 19-21%-2,6, Type 2, STI 8207
 79-81%-2,4, Type 1, STI 8207
 79-81%-2,4, Type 2, STI 8207

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC PREMINOL® S 1004F Polyol
BASF Lupranate® 259 Isocyanate
BASF Lupranate® 253 Isocyanate
BASF Lupranate® 245 Isocyanate
BASF Lupranate® 277 Isocyanate

PBASG0705 / 132338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.