MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Astro Met Macor® Machinable Glass Ceramic
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic

Material Notes: General Description:

Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro Met, Inc. High dielectric strength makes Macor an excellent insulator. No out-gassing, essentially zero porosity and low helium permeation make it useful in vacuum applications. Because it is thermally stable and has thermal expansion characteristics similar to metals, it can be used where high heat and flame are problems. It can be sealed, metallized and brazed. Macor can be turned, milled, drilled, tapped, sawed and ground by ordinary metalworking tools and techniques. It is machined with high-speed steel or, more easily, with carbide tooling at relatively low speeds and feeds, but with greater depth of cut than is usual with metals. Use of a water-soluble coolant is recommended. The "chips" are a fine powder, easily controlled by coolant or vacuum. Because Macor is so readily machined, it is a cost effective material for small volume manufacturing and for developing ceramic prototypes which in production are made by pressing and sintering large quantities. It has been used for nozzles, sensor housings, bearings, fixtures, guides, electrical insulators, thermal isolators and numerous other applications where the unique technical properties of Macor provide a solution to a challenging materials problem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.52 g/cc
Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 250
Flexural Strength 15000 psi
Compressive Strength 50000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
Dielectric Strength 1000 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 1000 °Cno load

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Macor® Machinable Glass Ceramic
Accuratus MACOR Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
CeramTec Ceramtape GC Glass Ceramic
Borosilicate Glass

CASTR04 / 632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.