MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offering excellent combination between mechanical properties and surface aspect. This grade is widely used for automotive part: outside mirror base plate. This product is available in black color and in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.72 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0025 cm/cm
Linear Mold Shrinkage, Transverse 0.0045 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 215 MPaASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 310 MPaASTM D790
Flexural Modulus 17000 MPaASTM D790
Izod Impact, Notched 215 J/mASTM D265
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 - 262 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 220 °CASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
INEOS Styrolution Luran® S 778T ASA
Avient OnForce™ LFT NN-60 LGF/000 Natural Nylon 66 with 60% Long Glass Fiber
Avient Nymax™ GF 1200 60 HS Natural A Nylon 66 with 60% Glass Fiber
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Conditioned, 60% Glass Filled

PRHOD582 / 137813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.