MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Applied Silicone 40044 High Consistency Rubber, 35 Durometer Peroxide Cure (HCRP 35), Implant Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Clear, High Strength

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 40
 35Typical
Tensile Strength >= 1000 psi
 1600 psiTypical
Elongation at Break >= 500 %
 700 %Typical
200% Modulus 0.100 ksi
@Strain 200 %
Tear Strength >= 60.0 pli
 150 pliTypical
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 116 °C
 
Descriptive Properties
Cure SystemPeroxide
Post Cure60 min200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® 9235 High Performance Silicone Solid Rubber
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Peroxide Cure

PNUSILA919 / 194588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.