MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inovyn 250SB Polyvinyl Chloride General Purpose - Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Made by suspension polymerization.

APPLICATIONS
Injection :
moldings with complex flow paths
Pressing : mixed with VC-VAc copolymers for gramophone records
Calendering : rigid films and sheets ; used in blend with a suspension resin with a higher K value
Blow molding : alone or mixed with resins with a higher K value : especially injection-blow molding of bottles
All applications : mixed with suspension resins with a higher K value, for easy gelling and increased productivity.

Information provided by SolVin.

SolVin is a predecessor company to Inovyn.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l<= 0.30 g/lISO 1269
Apparent Bulk Density 0.590 g/cc0.0213 lb/in³ISO 60
Particle Size 63 µm63 µm>80% greater than value; ISO 1624
 250 µm250 µm<2% greater than value; ISO 1624
Viscosity Test 61 cm³/g0.61 dl/gReduced viscosity, K value = 50; ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Inovyn 263RB Polyvinyl Chloride General Purpose - Rigid
Inovyn 257RF Polyvinyl Chloride General Purpose - Rigid
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid
Inovyn 264GC Polyvinyl Chloride General Purpose - Rigid or Plasticized
Inovyn 258RD Polyvinyl Chloride General Purpose - Rigid

PSOLVI09 / 68369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.