MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP1200LV Casting Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the requirements of UL Standard 94 for a horizontal burn rating at 1/4" thickness. It was especially formulated to a 1:1 mix ratio for use in MMD equipment or side-by side cartridges. It contains abrasive aluminum oxide filler which can introduce wear considerations for wetted components. It shows very good stability in side-by-side cartridges. Cure is normally achieved at room temperature although an elevated cure schedule can be used to reach final properties quickly. This product was designed to be cured in less than 2 hours at 65oC for ease of processing and also to reduce viscosity. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. Times and temperatures from 2 hours at 65oC to 10 minutes at 100oC are typical for small castings (less than 100 grams).

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.56 g/ccPart A; TM R050-16
 1.63 g/ccMixed; TM R050-16
 1.70 g/ccPart B; TM R050-16
Water Absorption 0.19 %
@Time 86400 sec
TM R050-35
Viscosity 8000 cPPart A, RVT, #6, 20 rpm.; TM R050-12
 16000 cPPart B, RVT, #6, 20 rpm.; TM R050-12
 25000 cP
@Shear Rate 1.00 1/s
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Tensile Strength at Break 1000 psiTM R050-36
Tensile Strength, Ultimate 1000 psiTM R050-36
Tensile Strength, Yield 250 psiTM R050-36
Elongation at Break 40 - 50 %TM R050-36
Tensile Modulus 10.0 ksiTM R050-36
Compressive Yield Strength 400 psiTM R050-38
Compressive Strength 6000 psiBreak; TM R050-38
 6500 psiUltimate; TM R050-38
Compressive Modulus 25.0 ksiTM R050-38
Adhesive Bond Strength 1100 psiLap Shear-Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+14 ohm-cm
Dielectric Constant 3.2
@Frequency 100000 Hz
 3.5
@Frequency 100 Hz
Dielectric Strength 400 V/mil
Dissipation Factor 0.020
@Frequency 100000 Hz
 0.030
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature <=1.00 °C
Below Tg
 171 µm/m-°C
@Temperature >=1.00 °C
Above Tg
Thermal Conductivity 0.400 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 1.00 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 24.0 - 72.0 hour
@Temperature 25.0 °C
Pot Life 15.0 - 20.0 min
 
Descriptive Properties
Appearanceblack liquid
Mix Ratio1:1Weight and Volume
Side-By-Side Cartridges CapableYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive

PRESL112 / 101526

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.