MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Flex® TPE D 4308 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Linear Mold Shrinkage 0.0118 cm/cm0.0118 in/inASTM D955
Melt Flow 5.3 g/10 min5.3 g/10 min(Condition L) ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40.440.410 sec; ASTM D-2240
Tensile Strength, Ultimate 10.1 MPa1460 psiASTM D412
Elongation at Break 310 %310 %ASTM D412
Flexural Modulus 0.261 GPa37.9 ksimethod 1, Proc.B; ASTM D-790
Tear Strength 81.6 kN/m466 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural
Dynasol Calprene® 401 Thermoplastic Rubber SBS Dry
CPT C-Flex® R70-190 Opaque Biocompatible TPE
Cast Stainless Steel CF8M, ASTM A351
Cast Stainless Steel CF8C, ASTM A351

PLA107 / 49568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.