MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Aptek DAT-A-THERM 1000 Electrically insulating urethane film
Categories: Polymer; Adhesive; Film; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% solid, fully crosslinked (C-staged), thermoset urethane polymer, which will not outgas, while in place and is suitable for high vacuum environments. The film exhibits outstanding reversion resistance and physical stability under long-term aging of high humidity and heat. The ultimate in thermal conductivity and overall performance can be achieved by bonding DAT-A-THERM 1000 film to device and conductivity and overall performance can be achieved by bonding DAT-A-THERM 1000 film to device and substrate with DIS-A-PASTE 2000A/B and 2001 PMF thermally conductive urethane adhesives. Both film and adhesive system are compatible in resin and filler technologies and have been designed to be used together.

Uniform filler distribution for consistent thermal dissipation capability throughput film segment; Controlled manufacturing process for a void free film; Low modulus/high elongation for minimum stress buildup under components; Low Tg-remains flexible to -70ºC; Exceeds NASA outgassing requirements for high vacuum environments; Typical film thicknesses, 0.004 to 0.006 in. Custom thicknesses available; Available in sheet or die-cut forms

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.96 g/ccASTM D1475
Moisture Absorption at Equilibrium 0.15 %Cured property; ASTM D570
Outgassing - Total Mass Loss 0.17 %Cured property at 125ºC at 10E-6 torr
Collected Volatile Condensable Material 0.010 %Cured property at 125ºC; at 10E-6 torr
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1050 psi
@Thickness 0.127 mm
Cured; ASTM D638
Elongation at Break 75 %
@Thickness 0.127 mm
Cured; ASTM D638
Tensile Modulus 2000 psi
@Thickness 0.127 mm
Cured; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+14 ohm-cmCured property; ASTM D257
Dielectric Constant 5.8
@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength 1000 V/mil
@Thickness 0.127 mm
Cured; ASTM D149
Dissipation Factor 0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1
 147 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2
Thermal Conductivity 0.00230 cal cm/sec-cm²-°C
Glass Transition Temp, Tg -70.0 °CCured property; JMTP P-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gypsum (CaSO4 - 2H2O)
Omnova Solutions Chemigum® P7400 Nitrile Elastomer
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound
Abatron AboCast 8103-20 High-Performance Dielectric Epoxy
Abatron AboCast 8103-30 High-Performance Dielectric Epoxy

PAPTEK19 / 24181

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.