MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omya OMYACARB® BP - LU Calcium Carbonate
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution.

Applications: A de-dusted filler that is ideal for joint compounds, unsaturated polyester, cementitious grouts, plasters, paints, plastics, and adhesives.

Information supplied by Omya North America.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.70 g/cc
Brightness 91 %Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.030 %Moisture Loss at 110°C % (dry)
Particle Size 24 µmMedian Diameter
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 174.5, 175.300, 178.3297
 
Descriptive Properties
Calcium Carbonate %98
Magnesium Carbonate %1
Retained in 325 mesh (dry), %9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omya OMYACARB® BP - AZ Calcium Carbonate
Omya OMYACARB® 3 - LU Calcium Carbonate
Omya OMYACARB® UF - FL Calcium Carbonate
Omya OMYACARB® 10 - AZ Calcium Carbonate
Omya OMYACARB® 8 - LU Calcium Carbonate

EOMYA924 / 5636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.