MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-32245 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-32245 is a high performance thermoplastic elastomer specifically designed for overmolding and multi-shot molding applications in the healthcare/medical segment. Medalist MD-32245 is a low hardness, low density, RoHS compliant grade suitable for injection.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Bondability; BPA Free, Good Adhesion; Good Colorability; Good Compression Set; Good Flexibility; Good Impact Resistance; Good Moldability; Good Processability; Good Sterilizability; High Elasticity; Low Density; Low Hardness; Low Specific Gravity

Uses: Bonding; Flexible Grips; Gaskets; Handles; Jackeitng; Medical Devices; Medical/Healthcare Applications; Overmolding; Pharmaceuticals; Rubber Replacements

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D792
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45ASTM D2240
Tensile Strength at Break 700 psiASTM D412
Tensile Stress at Strain 220 psi
@Strain 100 %
ASTM D412
 320 psi
@Strain 200 %
ASTM D412
 425 psi
@Strain 300 %
ASTM D412
Elongation at Break 600 %ASTM D412
Tear Strength 145 pliASTM D624
Compression Set 18 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 540 - 575 °FMelt, Injection
Rear Barrel Temperature 380 - 420 °FInjection
Middle Barrel Temperature 500 - 540 °FInjection
Front Barrel Temperature 520 - 560 °FInjection
Nozzle Temperature 540 - 575 °FInjection
Zone 1 380 - 420 °FExtrusion
Zone 2 480 - 520 °FExtrusion
Zone 3 500 - 540 °FExtrusion
Zone 5 520 - 560 °FExtrusion
Die Temperature 520 - 560 °FExtrusion
Mold Temperature 70.0 - 100 °FInjection
Drying Temperature 140 °FInjection
Dry Time 2.00 - 4.00 hourInjection
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-34065 Thermoplastic Elastomer
Teknor Apex Medalist® MD-34040 Thermoplastic Elastomer

PTEKNQ0720 / 237211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.