MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Iupilon® GS 2010MN1 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: 10% glass fiber. Glass fiber reinforced (flame retardant) grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics. Superior impact strength. Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC. Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Water Absorption 0.14 %
@Temperature 23.0 °C
Immersion
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.0 MPaISO 527-1,2
Elongation at Break 2.9 %ISO 527-1,2
Tensile Modulus 4500 MPaISO 527-1,2
Flexural Strength 135 MPaISO 178
Flexural Modulus 4000 MPaISO 178
Charpy Impact Unnotched 55.0 kJ/m²ISO 179-1,2
Charpy Impact, Notched 10.0 kJ/m²ISO 179-1,2
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 100 - 175 VUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 67.0 µm/m-°CISO 11359-2
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 140 °CISO 75-1,2
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
@Thickness 0.750 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupilon® GS 2020MN1 Polycarbonate
Mitsubishi Iupilon® CGH 1020KR Polycarbonate
Mitsubishi Iupilon® EGN 2020BR Polycarbonate
Mitsubishi Iupilon® EGN 2020DF Polycarbonate
Mitsubishi Iupilon® EGN 2020DR 9913A Polycarbonate

PMITSU9224 / 191897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.