MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® GC-0710 ABS/PET, Unreinforced Recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Eco-friendly Post-Consumer recycled PET.

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 96ASTM D785
Tensile Strength, Yield 410 kg(f)/cm²50 mm/min; ASTM D638
Elongation at Break 40 %50 mm/min; ASTM D638
Flexural Strength 60.8 MPa2.8 mm/min; ASTM D790
Flexural Modulus 19100 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 12.0 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 28.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 94.0 °CB/50; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm
 
Optical PropertiesOriginal ValueComments
Yellow Index 25 %
@Thickness 3.20 mm
ASTM D1925

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® GC-0703 ABS/PET, Unreinforced Recycled
Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled
Avient Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)
A. Schulman Diamond DIAMALOY ABSPC 750 HF ABS/PC Alloy, Non-Halogen, Flame Retardant
A. Schulman Diamond DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE

PSAMSU740 / 146557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.