MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
North American Quaking Aspen (Trembling Aspen) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)/Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Interior joinery, Matches

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Populus tremuloides; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 g/ccOven Dry Weight/Unseasoned Volume
 0.380 g/ccAir Dry (12-15% Moisture Content)
 43.0 lb/ft³Unseasoned*
Cell Length 1.00 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1200 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1400 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1600 NSide
Tensile Strength, Ultimate 1.80 MPaPerpendicular to Grain
 180 psiPerpendicular to Grain*
Modulus of Rupture 0.0580 GPaStatic Bending
 5.30 ksiStatic Bending*
Flexural Yield Strength 2900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 8.10 GPaStatic Bending
 840 ksiStatic Bending*
Compressive Strength 2.60 MPaPerpendicular to Grain
 29.0 MPaParallel to Grain
 200 psiPerpendicular to Grain*
 1620 psiParallel to Grain*
 2160 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.022µTL, 12% Moisture Content
 0.054µRL, 12% Moisture Content
 0.374µLT, 12% Moisture Content
 0.489µLR, 12% Moisture Content
 0.496µTR, 12% Moisture Content
Machinability 50 %Medium Relative to Other Wood
Shear Strength 5.90 MPaOrientation Unknown
 620 psiParallel to Grain*
Impact 2.5in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 6900psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.650 in-lb/in³Static Bending*
Work to Maximum Load 6.90 in-lb/in³Static Bending*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.670 BTU-in/hr-ft²-°FOven Dry
 0.800 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.5 %Radial; Green to Zero Moisture
 6.7 %Tangential; Green to Zero Moisture
 11.5 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorGrey, white to pale brown Usual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Largetooth Aspen (Bigtooth Aspen) Wood
American Balsam Fir Wood
North American Engelmann Spruce Wood
American Eastern White Pine Wood
American Ponderosa Pine Wood

PTSA140 / 71252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.