MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grades. This can, of course, raise the cost of toolmaking. Due to the very carefully balanced alloying and the powder metallurgical manufacturing route, Uddeholm Vanadis 6 has a similar hardening procedure as the common cold work tool steel. In order to reduce the amount of retained austenite and to optimize the abrasive wear resistance high temperature tempering is recommended. One very big advantage with Uddeholm Vanadis 6 is that the dimensional stability after hardening and tempering is much better than for conventionally produced cold work steel and HSS used for cold work. This also means that Uddeholm Vanadis 6 is a tool steel which is very suitable for CVD and PVD coating

Vanadis 6 is characterized by:

  • Very high abrasive-adhesive wear resistance
  • High compressive strength
  • Good toughness
  • Very good dimensional stability at heat treatment and in service
  • Very good through-hardening properties
  • Good resistance to tempering back
  • High cleanliness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.270 lb/in³hardness of 60 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 255Soft annealed
Hardness, Rockwell C 60Hardened and tempered
Modulus of Elasticity 32600 ksi(hardness of 60 HRC)
 27500 ksi
@Temperature 399 °C
hardness of 60 HRC
 30400 ksi
@Temperature 199 °C
hardness of 60 HRC
Compressive Yield Strength 2290 MPa0.2%, hardness of 60 HRC, tempered at 977°F 2 + 2h.
 2530 MPa0.2%, hardness of 62 HRC, tempered at 977°F 2 + 2h.
 2760 MPa0.2%, hardness of 64 HRC, tempered at 977°F 2 + 2h.
Impact Test 13.5 ft-lbhardness of 62 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.20 µin/in-°F
@Temperature 199 °C
hardness of 60 HRC
 6.70 µin/in-°F
@Temperature 399 °C
hardness of 60 HRC
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 20.0 °C
hardness of 60 HRC
Thermal Conductivity 22.0 W/m-K
@Temperature 199 °C
hardness of 60 HRC
 25.0 W/m-K
@Temperature 399 °C
hardness of 60 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.1 %
Chromium, Cr 6.8 %
Iron, Fe 82.8 %As Balance
Manganese, Mn 0.40 %
Molybdenum, Mo 1.5 %
Silicon, Si 1.0 %
Vanadium, V 5.4 %
 
Descriptive Properties
Pin-On-Disc Wear3.3 mg/min62HRC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Assab Steels VANADIS 10 Cold Work Steel
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel

NBUCOR07 / 15476

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.