MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, potting, tool-making, and many other applications. MPG-A25A is designed for an easy operation for industrial applications without special casting or heating equipment. The mixing ratio between part-A (MPG-062) and part-B (PPA-059) is 1:1 by volume. The material is specially formulated to be less moisture sensitive for relatively uncontrolled processing environments. Its low viscosity also makes it easy to achieve replicating the details of the mold/original with a fine resolution. Urethane elastomer parts made of this system exhibit:
  • Fine resolution of mold details
  • Highly flexible finish for easy demolding of parts
  • Good resiliency and elongation for easy demolding of parts
  • Good cut/tear resistance for its class
  • Good performance in wet environments

The suitable applications of MPG-A25A include stamps/patterns and concrete molds designed to transfer a decorative image to wet surfaces. This material is recommended specially for making patterns with high degree of under cuts.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 27ASTM D2240
Tensile Strength 311 psiASTM D412
Elongation at Break 291 %ASTM D412
Tear Strength 20.0 pliSplit; ASTM D624
 61.0 pliDie-C; ASTM D624
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 95.0 °FPrepolymer Temperature
 70.0 - 95.0 °FCuring Agent Temperature
Mold Temperature 70.0 - 95.0 °F
Cure Time 5.00 - 8.00 hour
@Temperature 25.0 °C
De-mold Time
 72.0 - 96.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 20.0 min
 
Descriptive Properties
Curing AgentPPA-059
PrepolymerMPG-062
Weight Ratio1:0.966Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Northstar Polymers MPP-A50A High Performance Polyether
Northstar Polymers MPP-A47A Liquid Castable Polyurethane
Northstar Polymers MPA-A30B Mold-Making Resin
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer

PNORTH838 / 162554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.