MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos R01A-00 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random copolymer R01A-00 is an antistatic polypropylene produced by a unique catalyst technology. It is designed for blow molding and extrusion applications and exhibits good stiffness and improved cycles. Product grade R01A-00 meets FDA requirements of 21CFR 177.1520.

Key Words: Good stiffness and improved cycles
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7676ASTM D785
Hardness, Shore D 6666ASTM D2240
Tensile Strength at Break 21.9 MPa3180 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 28.1 MPa4070 psi2.0 in/min; ASTM D638
Elongation at Break 680 %680 %2.0 in/min; ASTM D638
Elongation at Yield 13 %13 %2.0 in/min; ASTM D638
Tensile Modulus 0.669 GPa97.0 ksiSecant at 1%; ASTM D638
Flexural Modulus, 1% Secant 986 MPa143000 psiASTM D790A
Izod Impact, Notched  0.374 J/cm
@Temperature 3.89 °C
0.700 ft-lb/in
@Temperature 39.0 °F
ASTM D256
 0.854 J/cm
@Temperature 22.8 °C
1.60 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  3.59 kJ/m²
@Temperature 3.89 °C
1.71 ft-lb/in²
@Temperature 39.0 °F
Area; ASTM D256
 8.30 kJ/m²
@Temperature 22.8 °C
3.95 ft-lb/in²
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FUnannealed; ASTM D648
Vicat Softening Point 133 °C271 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 57 %
@Thickness 1.27 mm
57 %
@Thickness 0.0500 in
ASTM D1003
Gloss 93 %93 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processBlow Molding
 Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos R01C-00 Polypropylene Random Copolymer
Ineos R01C-01 Polypropylene Random Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Ineos R05C-00 Polypropylene Random Copolymer

PINEOS008 / 48176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.